pad-weld 2.5mm 7018 hand back in after 2yrs

Liste des GroupesRevenir à sej welding 
Sujet : pad-weld 2.5mm 7018 hand back in after 2yrs
De : null (at) *nospam* void.com (Richard Smith)
Groupes : sci.engr.joining.welding
Date : 03. Jul 2024, 08:36:40
Autres entêtes
Organisation : BWH Usenet Archive (https://usenet.blueworldhosting.com)
Message-ID : <m1v81n3p13.fsf@void.com>
User-Agent : Gnus/5.13 (Gnus v5.13)
Hi there

Glad I got a pack of 2.5mm 7018's from local stockist.

After two years, apart from one quick job - brings it all back.  Usual
fall-back - do pad-welds until "it's like riding a bicycle" - it
becomes automatic again.

Offcut of 10mm thickness plate - just right.
Cheap as cost per amount metal deposited and 2.5's leave small weld;
slow so forced to concentrate and control weld-pool; not natural match
to plate thickness (plate thicker than matches electrode size) so have
to concentrate on weld-pool control; no natural guide (get when doing
T-fillet) so ruling chalk-lines and following adds to skill and
control challenge.
Etc.

Amazing how much comes back to you.

Anyone else experience the like?

Best wishes,
Rich S

Date Sujet#  Auteur
3 Jul 24 * pad-weld 2.5mm 7018 hand back in after 2yrs2Richard Smith
3 Jul 24 `- Re: pad-weld 2.5mm 7018 hand back in after 2yrs1Jim Wilkins

Haut de la page

Les messages affichés proviennent d'usenet.

NewsPortal