   My neighbor has asked me to build up a worn spot on the drive pin of his framing nailer . I'm not sure what model it is . The pin has wear on the flat side at the tip , and it appears to be from sliding against the head of the next nail in line . I'm considering using SS for better abrasion resistance . The pin is not particularly hard , can be marked with a file , but "mushrooming" in the repaired area is also a consideration . Replacement pins are available ...
--
Snag
  Illegitimi non carborundum

Date Sujet#  Auteur
23 Jul 24 * 309SS or ER70S69Snag
23 Jul 24 +* Re: 309SS or ER70S65Jim Wilkins
23 Jul 24 i`* Re: 309SS or ER70S64Snag
23 Jul 24 i `* Re: 309SS or ER70S63David Billington
23 Jul 24 i  +- Re: 309SS or ER70S61Jim Wilkins
23 Jul 24 i  `- Re: 309SS or ER70S61Snag
23 Jul 24 `* Re: 309SS or ER70S63Bob La Londe
23 Jul 24  `* Re: 309SS or ER70S62Snag
23 Jul 24   `- Re: 309SS or ER70S61Jim Wilkins